LOCTITE EA 9392

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9392 AERO Epoxy Adhesive

Main features

  • 1,000 psi Aluminum Lap Shear
  • Thixotropic Gap-Filling Control
  • 75-Minute Working Window

Product Description

LOCTITE® EA 9392 AERO Epoxy Paste Adhesive is a two-component, room-temperature-curing epoxy paste adhesive for durable bonded assemblies. The thixotropic material supports gap-filling and potting applications while remaining workable for 75 minutes at 77°F/25°C when evaluated as a 100 g mass. It develops handling strength after 24 hours at 77°F/25°C and may be fully cured at room temperature or with an accelerated thermal schedule. Testing on prepared 2024-T3 aluminum demonstrates tensile lap shear performance across temperatures from -67°F/-55°C to 350°F/177°C, with 1,000 psi/6.9 MPa retained at the upper test temperature.

Key features

  • Elevated-temperature shear performance: Retains 1,000 psi/6.9 MPa tensile lap shear strength at 350°F/177°C under ASTM D1002 test conditions.
  • Thixotropic epoxy paste: Supports gap filling and potting while limiting uncontrolled flow during application.
  • Flexible cure scheduling: Cures in 5–7 days at 77°F/25°C or in 1 hour at 180°F/82°C for small adhesive masses.

Applications / Suitable for

  • Bonded assemblies requiring room-temperature cure
  • Gap-filling adhesive applications
  • Potting applications
  • Applications evaluated for shear strength at elevated temperatures

Technical Specifications

Physical Properties
Viscosity (Part A)
420,000 mPa.s
Viscosity (Part B)
660,000 mPa.s
General Properties
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:32

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material and processing properties. Component identities and test conditions are retained where relevant.

Property Value Unit Method / condition
Product type Two-component epoxy paste adhesive — As supplied
Rheology Thixotropic — Uncured material
Color — Part A Gray — Visual
Color — Part B Amber — Visual
Color — mixed Gray — After mixing Parts A and B
Viscosity — Part A 4,200 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity — Part A 420 Pa·s 25°C; Brookfield HBT, spindle 7 at 2.1 rad/s
Viscosity — Part B 6,600 Poise 77°F; Brookfield HBT, T-bar C at 5 rpm
Viscosity — Part B 660 Pa·s 25°C; Brookfield HBT, spindle 6 at 0.5 rad/s
Density — Part A 1.37 g/ml Uncured component
Density — Part B 1.0 g/ml Uncured component
Density — mixed 1.29 g/ml Parts A and B combined
Mix ratio by weight — Part A : Part B 100 : 32 parts Weight basis
Mix ratio by volume — Part A : Part B 100 : 44 parts Volume measurement is not recommended for structural applications unless ratio-control precautions are used
Pot life 75 minutes 100 g mass at 77°F/25°C; ASTM D2471 in water bath
Handling-strength time 24 hours At 77°F/25°C; full bond strength has not yet developed
Room-temperature cure 5–7 days At 77°F/25°C for normal performance
Accelerated complete cure 1 hour At 180°F/82°C; small masses only
Maximum stated accelerated-cure temperature 200 / 93 °F / °C Accelerated curing; small masses only
Maximum recommended mixed quantity 450 g Do not mix larger quantities because dangerous exothermic heat buildup may occur
Shelf life — Part A 1 year Stored below 40°F/4°C
Shelf life — Part B 1 year Stored below 40°F/4°C
Shelf life — Part A 1 year Stored below 77°F/25°C
Shelf life — Part B 1 year Stored below 77°F/25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive and bonded-joint results. Cure schedule, substrate preparation, test temperature and test method are retained because they materially affect interpretation.

Property Value Unit Method / condition
Tensile lap shear strength at -67°F/-55°C 3,500 / 24.1 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 77°F/25°C 4,300 / 29.6 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 180°F/82°C 2,500 / 17.2 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 250°F/121°C 2,000 / 13.8 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 300°F/149°C 1,300 / 9.0 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Tensile lap shear strength at 350°F/177°C 1,000 / 6.9 psi / MPa ASTM D1002; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Blister shear strength at -67°F/-55°C 3,000 / 20.7 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 77°F/25°C 4,000 / 27.6 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 180°F/82°C 2,500 / 17.2 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 250°F/121°C 2,000 / 13.8 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
Blister shear strength at 300°F/149°C 1,000 / 6.9 psi / MPa ASTM D3165; 2024-T3 bare FPL-etched aluminum; cured 7 days at 77°F/25°C
T-peel strength at 77°F/25°C 20 / 89 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 5 days at 77°F/25°C
Bell peel strength at 77°F/25°C 40 / 178 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 7 days at 77°F/25°C
Bell peel strength at 180°F/82°C 30 / 133 lb/in / N/25 mm ASTM D1876; 2024-T3 bare PAA aluminum; cured 7 days at 77°F/25°C
Service temperature based on retained lap shear Approximately 350 / 177 °F / °C Defined as the temperature at which 1,000 psi/6.9 MPa is retained under ASTM D1002
Tensile strength at 77°F/25°C 6,000 / 41.3 psi / MPa ASTM D638; 0.125 in/3.18 mm cast specimen
Tensile modulus at 77°F/25°C 475 / 3,273 ksi / MPa ASTM D638; 0.125 in/3.18 mm cast specimen
Elongation at break at 77°F/25°C 4 % ASTM D638; 0.125 in/3.18 mm cast specimen
Glass-transition temperature — dry 164 / 73 °F / °C Cured 7 days at 77°F/25°C
Glass-transition temperature — wet 144 / 62 °F / °C Cured 7 days at 77°F/25°C; immersed in 77°F/25°C water until equilibrium
Glass-transition temperature — dry, accelerated cure 356 / 180 °F / °C Cured 1 hour at 180°F/82°C
Compressive strength at 2% offset 9,300 / 64.1 psi / MPa ASTM D695 at 77°F/25°C; 1.15 in/29.2 mm diameter × 1 in/25.4 mm cylindrical specimens; cured 7 days at 77°F/25°C

Leading Brands Trust in Our Products and Services