ECCOBOND FP4531
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Snap cure
- Fast flow
- Passes NASA outgassing
Product Description
LOCTITE® ECCOBOND FP4531 underfill is designed for flip chip on flex applications with a 1mil gap. It is a snap curable epoxy with fast flow that passes NASA outgassing standards.
LOCTITE® ECCOBOND FP4531 is 62% filled, offers a pretty long pot life and has limited impurities. Its snap cure schedule can vary based on customer's experience and application requirements.
Snap Cure Schedule
- 7 minutes @ 160°C
Packaging
Unit of measure Syringe
Net weight 6.5 g
Gross weight 23 g
Dimensions 2 x 10.5 x 3.2 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Pot Life
24 hours
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed.
It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
Thermal Properties
Glass Transition Temperature (Tg)
161 °C
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding.
The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
Thermal Conductivity
0.61 W/m.K
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance.
Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
Physical Properties
Viscosity
10,000 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application