ECCOBOND FP4460

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond FP4460

Main features

  • Improved work life
  • High temperature performance
  • High flow

Product Description

LOCTITE® ECCOBOND FP4460 encapsulant is a silica filled, anhydride material designed for the protection of bare semiconductor devices. It is a low stress, low shrinkage and high flow oven cure product that is considered a glob top version of FP4450 with good ionic purity.

LOCTITE® ECCOBOND FP4460 has no JEDEC rating but its pressure pot performance on live devices is up to 500 hours with no failures, depending on device and package type.

Cure Schedule

  • 3 hours @ 150°C
Product Family

221965

10 cc - Syringe | Black
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Syringe
Net weight 17 g
Gross weight 27 g
Dimensions 2 x 10.5 x 3.2 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
48 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.78
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
173 °C
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
66.9 kV/mm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
425,000 mPa.s

Additional Information

We have internal information showing that these legacy semiconductor liquids pass UL94HB at 1/8” thickness but do not have the test data or yellow card nor are we going to test for it. This is anecdotal but, hopefully, helpful.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers