DOWSIL 1-4174
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Controlled 180 um Bondline
- 1.8 W/(m K) Thermal Conductivity
- 20-Minute Cure at 150 deg C
Product Description
DOWSIL 1-4174 Thermally Conductive Adhesive is a one-part, gray silicone adhesive for bonding and transferring heat between electronic components and thermal-management hardware. The self-leveling, self-priming material uses 180 um glass spacer beads for bondline control. Cure schedules are 90 minutes at 100 deg C, 30 minutes at 125 deg C, or 20 minutes at 150 deg C. Typical thermal conductivity is 1.8 W/(m K), and typical unprimed aluminum lap shear is 4.5 MPa. Applications include integrated circuits, lids and housings, baseplates, and heat sinks.
Key features
- Glass-bead bondline control: Embedded 180 um glass spacer beads control adhesive bondline thickness.
- Thermal conductivity: Typical thermal conductivity is 1.8 W/(m K).
- Elevated-temperature cure: The shortest listed cure schedule is 20 minutes at 150 deg C.
Applications
Bonding and sealing integrated circuits, lids and housings, baseplates, and heat sinks where thermal transfer is required.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Thermal Properties
Additional Information
DOWSIL™ 1-4174 One-Part Thermally Conductive Adhesive
DOWSIL™ 1-4174 is a one-part, gray, thermally conductive silicone adhesive formulated for electronic assemblies and thermal management applications. The adhesive can flow, fill, or self-level after dispensing without requiring the mixing of separate components. Its temperature-controlled heat-curing process produces no cure by-products, supporting uniform cure in deep sections and confined assemblies.
With a typical cured thermal conductivity of 1.78 W/mK and the ability to achieve thin bond line thicknesses, DOWSIL™ 1-4174 helps transfer heat away from electronic devices. Its 7 mil glass bead technology supports controlled bond line thickness, while its cured mechanical and electrical properties make it suitable for consideration in electronic bonding applications.
Thermal Performance, Bonding Strength & Processing Flexibility
DOWSIL™ 1-4174 combines thermal conductivity with adhesive bonding and temperature-controlled curing. Its one-part formulation and cured properties support the integration of thermal management and mechanical attachment within electronic assemblies.
Where DOWSIL™ 1-4174 Fits
DOWSIL™ 1-4174 is highly recommended for a range of electronic assembly bonding applications, including the attachment of components and structures involved in thermal management.





Typical As-Supplied & Cured Properties
Typical As-Supplied Properties
| Property | Typical Value | Method / Condition |
|---|---|---|
| Color | Gray | As supplied |
| Viscosity | 62,300 cP | Typical uncured value |
| Thixotropy | 3.7 | Typical uncured property |
| Specific Gravity | 2.71 | Uncured material |
| Heat Cure Time | 90 mins | 100°C |
| Heat Cure Time | 30 mins | 125°C |
| Heat Cure Time | 20 mins | 150°C |
| Rheometer T90 Cure Time | 6.2 min | 125°C |
Typical Cured Properties
| Property | Typical Value | Method / Condition |
|---|---|---|
| Thermal Conductivity | 1.78 W/mK | Typical cured property |
| Lap Shear Strength | 4.5 MPa | Aluminum substrate |
| Durometer Hardness | 92 Shore A | Cured material |
| Dielectric Strength | 400 V/mil | Electrical property |
| UL Flammability | UL 94 V-0 | Classification |
Temperature-Controlled Heat-Cure Processing
DOWSIL™ 1-4174 contains all ingredients required for cure. The addition-cure silicone process is initiated by heat and can be accelerated by increasing the curing temperature. The formulation provides a long working time before cure initiation and produces no cure by-products.
Typical Heat-Cure Schedule
Application & Curing Instructions
- Apply the adhesive to the prepared substrate and assemble the components.
- Heat cure at 100°C (212°F) or higher to initiate the addition-cure silicone curing process.
- Use higher curing temperatures when faster processing is required, following the applicable cure schedule.
- For thin bond lines of less than 20 mils, cure for approximately 15 minutes at 150°C (302°F).
- For thicker sections, perform a pre-cure at 70°C (158°F) to help minimize void formation.
- Use 30 minutes at 70°C (158°F) as a starting pre-cure condition, then optimize according to section thickness and the degree of confinement.
- Complete the final heat cure to achieve full adhesive properties and uniform curing throughout the material.
Cure Characteristics
- Contains all ingredients required for cure.
- Produces no cure by-products.
- Suitable for deep-section and confined applications.
- Cures uniformly throughout the adhesive.
- Provides a long working time before cure initiation.
Adhesion to Common Substrates
DOWSIL™ 1-4174 is formulated to provide unprimed adhesion to many reactive metals, ceramics, and glass, as well as selected laminates, resins, and plastics. The supplied substrate guidance also identifies epoxy laminate boards, reactive materials, and filled plastics among suitable substrate categories. Adhesion depends on substrate characteristics, and good adhesion is generally not expected on non-reactive metal surfaces or non-reactive plastics such as PTFE, polyethylene, and polypropylene.
| Substrate Type | Typical Adhesion Expectation |
|---|---|
| Reactive metals | Good unprimed adhesion |
| Ceramics | Good unprimed adhesion |
| Glass | Good unprimed adhesion |
| Selected laminates | Good adhesion |
| Selected resins | Good adhesion |
| Selected plastics | Good adhesion |
| Non-reactive metals | Adhesion may be limited |
| Teflon™ (PTFE) | Adhesion may be limited |
| Polyethylene | Adhesion may be limited |
| Polypropylene | Adhesion may be limited |
Substrate Testing & Improving Adhesion
The guidance identifies 100 percent cohesive failure of the adhesive in a lap shear or similar adhesive strength test as the criterion for maximum bond strength and substrate compatibility assessment.
Testing can also help determine minimum cure time and identify surface contamination from mold release agents, oils, greases, and oxide films.
Difficult or non-reactive substrates may benefit from chemical etching or plasma treatment to create a more reactive surface and promote adhesion.
A Dow primer may be used to increase the chemical activity of difficult substrates.
- Apply a very thin, uniform coating.
- Wipe off excess primer.
- Allow the primer to cure thoroughly before applying the silicone elastomer.
Increasing the cure temperature and/or cure time may improve ultimate adhesion where necessary. Conduct a small-scale laboratory evaluation of the substrate before proceeding to production trials.
Storage Instructions & Temperature Considerations
Store DOWSIL™ 1-4174 in its original packaging with the cover tightly attached to avoid contamination.
Follow any special storage instructions listed on the product label. Use the product by the indicated Expiration Date shown on the label.
Silicone adhesive performance at temperature extremes depends on the application, component configuration, stress sensitivity, cooling rates, hold times, and prior temperature history. Thermal cycling performance should be verified for the intended parts or assemblies.
At elevated temperatures, the durability of the cured silicone elastomer is dependent on both time and temperature.