CONATHANE EN-21

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CONATHANE EN-21

Main features

  • Low-viscosity
  • Room-temperature cure
  • Good electrical and thermal properties

Product Description

CONATHANE® EN-21 Polyurethane Encapsulant is a two-component, unfilled, low-viscosity polyurethane potting compound for electronic circuits, components, and power devices. The system supports hand-mix, meter-mix, and vacuum potting or casting processes and may cure at room temperature or with low-temperature heat. Documented applications include transformers, coils, reed and mercury switches, inductors, ignition systems, voltage regulators, ballasts, microcircuits, rectifiers, and printed circuit assemblies. Typical cured properties include Shore A 80 hardness, 155% elongation, 0.3 W/m·K thermal conductivity, moisture resistance, and thermal-shock performance.

Key features

  • Low-viscosity processing: Typical initial mixed viscosity is 2,000 cP at 25°C.
  • Room-temperature or heat cure: Recommended cure options are seven days at 25°C or four hours at 80°C.
  • Electrical and thermal properties: Typical data include 650 V/mil dielectric strength and 0.3 W/m·K thermal conductivity.

Applications / Suitable for

  • Transformers, coils, switches, and inductors
  • Voltage regulators, ballasts, and rectifiers
  • Microcircuits and printed circuit assemblies

Technical Specifications

General Properties
Color
Clear Amber / Clear Amber
Component System
Two (Urethane Prepolymer / Curative)
Specific Gravity
1.14 / 0.96
Electrical Properties
Dielectric Strength
25.6 kV/mm
Volume Resistivity
7.2 x 10¹⁴ Ohms⋅cm
Chemical Properties
Water Absorption
0.07 %
Thermal Properties
Thermal Conductivity
0.3 W/m.K

Additional Information

Two-Component Polyurethane Potting Compound

CONATHANE EN-21

CONATHANE EN-21 is a two-component, unfilled, low-viscosity polyurethane potting compound designed for electronic encapsulation, casting, embedding, and potting applications. Its low viscosity allows the material to flow around complex electronic components and into narrow spaces during encapsulation.

Cured CONATHANE EN-21 provides electrical insulation, moisture resistance, and thermal shock resistance while maintaining low exotherm and low shrinkage during cure. The material is formulated specifically for electronic circuits, components, and power devices.

100:116 mix ratio by weight 2,000 cP initial mixed viscosity at 25 °C 650 V/mil dielectric strength UL 94 HB at 25 °C
Two metal cans of CONATHANE EN-21 two-component polyurethane potting compound, labeled Part A and Part B.
Polyurethane potting compound for electronic encapsulation and casting applications
Key Features

Low-viscosity encapsulation with electrical and environmental protection

Low-Viscosity Polyurethane System

Facilitates material flow around closely spaced components and complex electronic assemblies for effective encapsulation. The material is unfilled and supports multiple potting and casting methods.

Electrical Insulation Properties

Provides a dielectric strength of 650 volts/mil according to ASTM D149 at 25 °C (77 °F), with a test thickness of 1/16 inch. Additional dielectric and electrical resistance properties are documented in the technical tables.

Moisture and Thermal Shock Resistance

Helps protect encapsulated electronic components from moisture exposure and stresses associated with temperature changes. The cured material passed 10 thermal shock cycles from -65 °C to 130 °C under MIL-I-16923E.

Flammability Rating and RoHS Compliance

UL flammability rating: CONATHANE EN-21 has a UL 94 HB flammability rating at 25 °C (77 °F).
RoHS compliance: Both Part A (urethane prepolymer) and Part B (curative) comply with the requirements of RoHS Directive 2011/65/EU, as amended by Directive (EU) 2015/863.
Technical Specifications

Typical properties of material as supplied and mixed

CONATHANE EN-21 is supplied as Part A urethane prepolymer and Part B curative. The specified mix ratio is 100 parts Part A to 116 parts Part B by weight.

Typical Properties of Material as Supplied

Property CONATHANE® EN-21 Part A
Urethane Prepolymer
CONATHANE® EN-21 Part B
Curative
Conditions / Test Method
Viscosity 6,000 cP 800 cP 25 °C / 77 °F
Specific Gravity 1.14 0.96 25 °C / 77 °F
Appearance Clear Amber Clear Amber —
Mix Ratio 100 116 Parts by weight
Flashpoint > 94 °C
> 201 °F
> 94 °C
> 201 °F
ASTM D93

Typical Properties of Mixed Material

Property Value Conditions
Viscosity (initial) 2,000 cP 25 °C / 77 °F
Viscosity (initial) 320 cP 60 °C / 140 °F
Pot Life 40 minutes 25 °C / 77 °F
Pot Life 8 minutes 60 °C / 140 °F
Gel Time 90 minutes 25 °C / 77 °F
Gel Time 20 minutes 60 °C / 140 °F
Electrical Performance

Typical Electrical Properties of Cured Material

Property Typical Value Test Method Conditions
Dielectric Strength 650 volts/mil ASTM D149 25 °C / 77 °F — 1/16”
Dielectric Constant 3.4 ASTM D150 1 kHz — 25 °C / 77 °F
Dielectric Constant 6.1 ASTM D150 1 kHz — 105 °C / 221 °F
Dissipation Factor 0.02 ASTM D150 1 kHz — 25 °C / 77 °F
Dissipation Factor 0.03 ASTM D150 1 kHz — 105 °C / 221 °F
Insulation Resistance > 2.5 × 1013 Ω MIL-M-24041C 25 °C / 77 °F
Insulation Resistance 1.4 × 109 Ω MIL-M-24041C 130 °C / 266 °F
Volume Resistivity 7.2 × 1014 Ω·cm ASTM D257 25 °C / 77 °F
Volume Resistivity 1.8 × 1011 Ω·cm ASTM D257 130 °C / 266 °F
Surface Resistivity > 1.0 × 1015 Ω ASTM D257 25 °C / 77 °F
Surface Resistivity 6.9 × 1012 Ω ASTM D257 130 °C / 266 °F
Physical and Thermal Performance

Typical Physical Properties of Cured Material

Property Typical Value Test Method Conditions
Shore Hardness A 80 ASTM D2240 25 °C / 77 °F
Tensile Strength 2,000 psi ASTM D412 25 °C / 77 °F
Ultimate Elongation 155% ASTM D412 25 °C / 77 °F
Tear Strength 120 pli ASTM D624 25 °C / 77 °F
Linear Shrinkage 1.4% — 25 °C / 77 °F
Water Absorption 0.07% ASTM D570 24 h @ 25 °C / 77 °F
Water Absorption 0.15% ASTM D570 7 d @ 25 °C / 77 °F
Water Absorption 0.16% ASTM D570 28 d @ 25 °C / 77 °F
Compression Set 10% ASTM D395 Method B 25 °C / 77 °F
Specific Gravity 1.07 — 25 °C / 77 °F
Coefficient of Thermal Expansion 210 ppm / °C ASTM D696 25 °C / 77 °F
Hydrolytic Stability pass MIL-M-24041C —
Thermal Conductivity 0.3 W / m·K ASTM C177 25 °C / 77 °F
Thermal Shock pass 10 cycles MIL-I-16923E -65 °C to 130 °C
UL Flammability Rating 94 HB UL 94 25 °C / 77 °F

Heat Stability of Cured Material — After Exposure at 130 °C / 266 °F

Property Before After Exposure Duration
Weight Loss - 0.34% 500 hours
Weight Loss - 0.48% 1000 hours
Shore Hardness A 80 A 91 500 hours
Shore Hardness A 80 A 96 1000 hours
Application Guidance

Application Methods and Curing Schedule

CONATHANE EN-21 supports several potting and casting methods. Parts A and B must be combined at the specified ratio by weight before application, followed by thorough mixing and degassing.

Application Methods

Hand-mix Bench Potting / Casting
Cartridge Dispensing
Meter-mix Bench Potting / Casting
Meter-mix Vacuum Potting / Casting

Mixing and Degassing

  1. Measure and combine EN-21 Part A and EN-21 Part B according to the specified 100:116 mix ratio by weight.
  2. Mix thoroughly using a metal or glass container and a metal or glass stirrer until a uniform mixture is achieved.
  3. Degas the mixture at room temperature under a vacuum greater than 27 inHg.
  4. Allow for froth by using a container large enough to accommodate expansion during the degassing process.

Recommended Curing Schedules

Room-Temperature Cure
7 days at 25 °C (77 °F)
OR
Elevated-Temperature Cure
4 hours at 80 °C (176 °F)

Start timing the cure only after the material has reached the specified curing temperature.

Verify curing conditions for the specific application, as the recommended cure schedules may need adjustment to achieve optimal performance.

Primer Recommendations

Primers are available if improved adhesion is required. The supplied application guidance recommends the following:

Additional Information

Shelf Life, Transportation, Storage, and Handling

Storage Conditions

Store between 20–30 °C / 68–86 °F in a dry controlled environment out of direct sunlight.

Shelf Life

This material should be suitable for use for twelve (12) months from the date of shipment when stored under the recommended conditions in the original sealed containers.

Moisture Sensitivity

This product is sensitive to moisture and atmospheric humidity. Containers, once opened, should be used immediately or blanketed with dry air or nitrogen before resealing.

Failure to store the product as recommended above may lead to deterioration in product performance.

Handling Precautions

Although the very low vapor pressure of these systems greatly reduces the vapor hazard as compared to TDI-based systems, careless handling of any isocyanate should be avoided. Avoid contact with the resins and hardeners. The use of protective clothing is recommended.

  • In case of skin contact, wash immediately with mild soap and water.
  • In case of eye contact, flush eyes immediately with water and obtain medical attention.
  • Use in well-ventilated areas and avoid prolonged or repeated breathing of vapors.
  • Accidental spills in the work area should be wiped up right away.

Review the component-specific safety data sheets for additional safety and handling information.

Recommended Applications

Electronic encapsulation, potting, and casting applications

CONATHANE EN-21 is formulated specifically for electronic circuits, components, and power devices. The following applications are identified in the supplied product information.

Electronic Circuits and PCB Assemblies

Coils and Switching Components

Regulation and Power Components

  • Voltage regulators and ballast
  • Rectifiers and micro-circuits
Featured Application

CONATHANE EN-21 for Smart Meter Electronics

Three smart utility meters with digital displays and white housings, showcasing modern smart metering technology.

 

Smart electricity, water, and gas meters rely on electronic assemblies that must operate reliably under varying environmental conditions. Moisture exposure and temperature fluctuations can affect sensitive components, potentially compromising meter performance and measurement accuracy.

CONATHANE EN-21 can be used to encapsulate printed circuit boards and electronic components within smart meters, including inductors, coils, and voltage regulators. By forming a protective barrier around these assemblies, the material helps reduce exposure to environmental conditions that could affect their long-term reliability.

Next Steps

Evaluate CONATHANE EN-21 for Your Electronic Potting Application

Share your electronic assembly requirements, component configuration, potting or casting method, processing conditions, and curing requirements to discuss CONATHANE EN-21 for electronic encapsulation, power components, printed circuit board assemblies, or smart-meter applications.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers