3M™ Hot Melt Adhesive 3748 V0

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Hot Melt Adhesive 3748V-0

Main features

  • Excellent adhesion
  • Good electrical properties
  • Non-corrosive to metal

Product Description

3M™ Hot Melt Adhesive 3748 V0 is a high-performance, 100% solids thermoplastic adhesive designed to deliver strong, flexible bonds across a range of demanding applications. Engineered for durability, it provides excellent peel adhesion, reliable thermal shock resistance, and superior heat resistance, making it well-suited for both electronic and general industrial uses.

This hot melt adhesive features outstanding electrical insulating properties, making it an ideal choice for bonding and securing components on printed wiring boards (PWBs) and other electronic assemblies. Its non-corrosive formulation ensures compatibility with metal components, helping maintain the integrity and longevity of sensitive parts.

A key advantage of 3M™ Hot Melt Adhesive 3748 V0 is its self-extinguishing property, supported by a UL 94 V-0 flammability rating. This makes it especially suitable for applications where flame resistance and safety compliance are critical. Beyond electronics, it is also widely used in industrial bonding and sealing applications where flexibility, toughness, and flame-retardant characteristics are required.

With its combination of strength, flexibility, and safety features, this adhesive provides a dependable solution for high-performance bonding in environments that demand reliability and protection.

Product Key Features

  • Tough, flexible thermoplastic hot melt adhesive with 100% solids formulation
  • Provides excellent peel adhesion and strong, durable bonds
  • Good thermal shock resistance and higher heat resistance
  • Excellent electrical insulating properties for electronic applications
  • Ideal for printed wiring boards and other electronic bonding uses
  • Self-extinguishing with UL 94 V-0 flammability rating
  • Suitable for industrial bonding and sealing applications requiring flame resistance
  • Non-corrosive to metal, ensuring compatibility with sensitive components
Product Family

234893

White, 15 mm x 200 mm, 5 kg
1. Select Package Type
2. Select Width
3. Select Length

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Box
Net weight 5.363 kg
Gross weight 5.363 kg
Dimensions 21.6 x 16.8 x 27.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Polyolefin
Color
The color
Light Yellow
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.09
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
3,300 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers